Pressless process used for the preparation of sintered Nd-Fe-B magnets has been studied. The effect of the average particle size D av, filling density ρf, and powder-texturing conditions for obtaining density ρ and desired magnetic hysteretic properties of sintered magnets has been investigated for both traditional technology (TT) and low-oxygen technology (LOT). The ρf magnitude ensuring the optimum relation between the density ρ of sintered magnets and their degree of texture was shown to be 2.5–3.0 and 2.2 g/cm3 for the TT and LOT, respectively. At lower ρf magnitudes, no required density of sintered magnets is reached, whereas at higher filling densities, a low level of texture and low remanence are realized. Optimum parameters of pulsed field inducing the high degree of texture in powders have been determined. The following properties were achieved for magnets prepared by pressless LOT: B r ≥ 14.2 kG, H c ≥ 8 kOe, and (BH)max ≥ 47.9 MG Oe.

Authors:   A. G. Popov, A. V. Shitov, E. G. Gerasimov, D. Yu. Vasilenko, M. Yu. Govorkov, D. Yu. Bratushev, V. P. Vyatkin, K. Yu. Shunyaev, T. L. Mikhailova
Journal:   The Physics of Metals and Metallography
Year:   2012
DOI:   10.1134/S0031918X12040096
Publication date:   16-04-2012

Watchlist

This is where you can add this publication to your personal favourites.

Additional Information

Facts, background information, dossiers
  • B&R
More about Springer-Verlag
Contact
Springer-Verlag GmbH
Tiergartenstraße 17
69121 Heidelberg
Germany
Phone
++49 / (0)6221 / 487-0
Fax
++49 / (0)6221 / 413982
Your browser is not current. Microsoft Internet Explorer 6.0 does not support some functions on Chemie.DE