ChemInform Abstract: Atomic Layer Deposition Synthesis of Platinum—Tungsten Carbide Core—Shell Catalysts for the Hydrogen Evolution Reaction.

Abstract

WC powders are prepared by solid state reaction of WO3 and carbon black at 1300 °C in the presence of KCl and a Ni catalyst.

Authors:   Hsu, Irene J.; Kimmel, Yannick C.; Jiang, Xiaoqiang; Willis, Brian G.; Chen, Jingguang G.
Journal:   ChemInform
Volume:   43
Issue:   19
Year:   2012
Pages:   no
DOI:   10.1002/chin.201219009
Publication date:   08-05-2012